Abstrakt

This paper discussed the effect of the addition of silica fume (2 wt.% and 4 wt.%) and alumina (2 wt.% and 4 wt.%) on the properties of fly ash geopolymer concrete. The fly ash geopolymer concrete achieved the highest 28-day compressive strength with 2 wt.% of silica fume (39 MPa) and 4 wt.% of alumina (41 MPa). The addition of 2 wt.% of silica fume increased the compressive strength by 105% with respect to the reference geopolymer (without additive). On the other hand, the compressive strength surged by 115% with 4 wt.% of alumina compared to the reference geopolymer. The addition of additives improved the compactness of the geopolymer matrix according to the morphology analysis.
Przejdź do artykułu

Autorzy i Afiliacje

Fong Sue Min
1
Heah Cheng Yong
1 2
ORCID: ORCID
Liew Yun Ming
1 3
ORCID: ORCID
Mohd Mustafa Al Bakri Abdullah
1 3
ORCID: ORCID
Hasniyati Md Razi
4
Foo Wah Low
5
Ng Hui-Teng
1 2
Ng Yong-Sing
1 2

  1. Centre of Excellence Geopolymer and Green Technology (CEGeoGTech), Universiti Malaysia Perlis (UniMAP), 01000 Perlis, Malaysia
  2. Faculty of Mechanical Engineering Technology, Universiti Malaysia Perlis (UniMAP), 02600 Perlis, Malaysia
  3. Faculty of Chemical Engineering Technology, Universiti Malaysia Perlis (UniMAP), 01000 Perlis, Malaysia
  4. Reactor Technology Center, Technical Support Division, Malaysian Nuclear Agency, Bangi, 43000 Kajang, Malaysia
  5. Department of Electrical & Electronic Engineering, Lee Kong Chian Faculty of Engineering & Science, Universiti Tunku Abdul Rahman, Bandar Sungai Long, 43000 Kajang, Malaysia

Ta strona wykorzystuje pliki 'cookies'. Więcej informacji