The gold recovery from cyanidation tailings was only 4.01% with the general flotation process, the surface analyses of flotation products were performed, and the results showed that the poor gold recovery with general flotation process was due to the passive films covering the surface of the gold bearing pyrite. These films are mainly hydrophilic hydroxides of Ca, Fe and Mg, at the same time, the depression of CN– to pyrite flotation in the flotation slurry was also a main contributing factor. With the surface repair regeneration procedures, it was proven that sulfuric acid pretreatment plays a dominant role in the removing and cleaning of passive films, while destroying free cyanides in the slurry. Sodium carbonate was then used as a buffering pH modifier and as a slurry dispersant after sulfuric acid pretreatment. The gold recovery was as high as 93.41%, compared to the original gold recovery of 4.01%.
Go to article

Authors and Affiliations

Huang Zhongsheng
1 2 3
Yang Tianzu
1

  1. School of Metallurgy and Environment, Central South University, Changsha 410083, Hunan, China
  2. State Key Laboratory of Comprehensive Utilization of Low-Grade Refractory Gold Ores, Xiamen 3361101, Fujian, China
  3. Zijin Mining Group Company Limited, Shanghang 364200, Fujian, China

This page uses 'cookies'. Learn more